Compents:Polymer ofglycerin,
epoxy propane and Epoxy ethane
Index:
Appearance: |
transparent liquid, no mechanical impurities |
Hydroxyl value(KOHmg/g) |
32-36 |
Acid value |
0.08 |
Moisture(%,≤) |
0.1 |
Viscosity(25¡æ)mPa.s |
650-1050 |
chromaticity(APHA,≤) |
100 |
MW |
5000 |
|
Usage£º |
This product is highly active polyether, high reactivity. Used for polyurethane molded foam (RIM) response to prepare high springback products, such as car cushions, steering wheel, instrument panel and handles, etc, with excellent recovery, compressibility and comfort. |
Package£º |
Galvanized barrels
, net weight 200KG per barrel |
storage and transportation£º |
storage in a dry environment at room temperature . Prevent rain during transportation and contamination. Sealed after usage to prevent moisture absorption. Storage period of six months from the date of production |
Safety and toxicity£º |
High flash point, flammable; non-explosive;put off with foam, dry powder, steam and water when fire. |
| |
|
|
|
|